[AR] Re: Amateur thermoplastic binder solids

  • From: "Troy Prideaux" <troy@xxxxxxxxxxxxxxxxxxxxx>
  • To: <arocket@xxxxxxxxxxxxx>
  • Date: Fri, 10 Jul 2020 10:53:49 +1000

Ben,
  All my melting and casting has been done with hybrid grains - no oxidizer. 
The thermal processing of the urethane based stuff (recently discussed) was 
always well below 100deg C ie. just enough to encourage the liberation of 
loitering moisture under vacuum conditions... well... to assist with the 
processing of mix as well.

Troy


Agreed that hands-off melting and casting seems like a good idea, but from
Troy it sounds like that is fairly well sorted out already.




Other related posts: