"no smoke"
Do you mean no aluminum?

On Tue, Jul 7, 2020 at 8:45 PM Ben Brockert <wikkit@xxxxxxxxx> wrote:

On Tue, Jul 7, 2020 at 8:19 PM Troy Prideaux <troy@xxxxxxxxxxxxxxxxxxxxx>
wrote:
  BUT, the catch is the processing. You need to invest in the processing
kit or get real clever with the chem.

Are you willing to go into any more detail, or is "process it at
temperatures and pressures that preclude the existence of water" the
crux of it? it being higher performance, full density, and no smoke
make me surprised that it isn't more common.

Thanks,
Ben